Gas-Shielded Flux Cored (Requires the use of an externally |
Self-Shielded Flux Cored (No shielding gas required. Good for outdoor windy conditions. Hotter than solid wires.) | |||
---|---|---|---|---|
Wire Size: |
Wire Size: |
|||
Wire Feed Speed*: |
Wire Feed Speed*: |
|||
Amperage Range: |
Amperage Range: |
|||
Shielding Gas & Voltage Range**: |
Voltage Range: |
|||
*Wire Feed Speed is a starting value only and can be fine-tuned while welding. **CO2 gas is economical and has deeper penetration on steel, but may be too hot for thin metal. 75% Argon / 25% CO2 is better on thin steels, produces less spatter and better bead appearance. Settings based on butt welds. Joint design, fitup, backup, position, bead size and stickout may alter conditions. |